Rust in the Throwing Shed
1The track and field team at Brookhaven Middle School keeps its throwing gear in a shed beside the field. After a wet spring, Coach Gretchen Albrecht found orange-brown rust on several iron shot puts. “Rust eats the iron away,” she said, so she expected the rusty shot puts to be lighter than new ones. Tobias Nakamura-Reyes, a seventh-grade shot putter, was not so sure. He took the question to his science teacher, Ms. Ifeoma Chukwu, and they planned a test with steel wool. Steel wool is mostly iron, and its thin strands rust much faster than a solid shot put.
2Ms. Chukwu gave Tobias a simple model of rusting: iron atoms combine with oxygen atoms from the air to form iron oxide. Water speeds up the reaction. The model can be written as 4 Fe + 3 O₂ → 2 Fe₂O₃. In this reaction, every 7.0 g of iron that rusts combines with 3.0 g of oxygen to form 10.0 g of iron oxide.
3Tobias pulled apart six pads of steel wool with the same dry mass, 5.00 g each. He dipped each pad in tap water and let it drip. Five pads went into open dishes on a lab shelf. On each test day, Ms. Chukwu took one of those pads, dried it in a warm oven and let it cool, and Tobias weighed it. The sixth damp pad went into a 1-liter glass jar, which they sealed with a tight lid. On each test day, Tobias weighed the whole jar with everything inside it, without opening it (Table 1).
4On day 14, they opened the jar. Only part of the pad inside had turned orange-brown; the rest of its strands were still gray and shiny. After drying, that pad had a mass of 5.28 g. Ms. Chukwu pointed out that 1 liter of air holds only about 0.28 g of oxygen. The pads in the open dishes, by contrast, were orange-brown almost all the way through.